Production process:
(1) Strict requirements for chemical composition, requiring a higher carbon and silicon content in the original molten iron compared to gray cast iron, reducing the content of manganese, phosphorus, and sulfur in ductile iron
(2) The discharge temperature of molten iron is higher than that of gray cast iron to compensate for the loss of molten iron temperature during spheroidization and inoculation treatment
(3) Perform spheroidization treatment by adding spheroidizing agents to the molten iron
(4) Add inoculant for inoculation treatment
(5) Ductile iron has poor flowability and large shrinkage, so it requires a higher pouring temperature and a larger pouring system size. Reasonable use of risers and chilled iron should follow the principle of sequential solidification
(6) Perform heat treatment

product details


7269d1eaf830d3a0687f4c1bf0f2834.png

694d790b61962c392111b622c0c1d3d.jpg

球墨 (1).jpg

球墨 (2).jpg

球墨 (3).jpg

球墨 (4).jpg

球墨 (5).jpg

球墨 (6).jpg

球墨 (7).jpg

球墨 (8).jpg

球墨 (9).jpg

球墨 (10).jpg


Previous page:It's already the first page
Next page:It's already the last page

For more information and quotations, please contact me immediately!

Submit

Related products